- Produktspezifikationen
- Verpackung
- Bitte um Angebot
SA 2594 has high intergranular-corrosion, pitting and stress-corrosion resistance with exceptional mechanical strength properties when welded with our high basic agglomerated flux FL 838.
1.4507, 1.4410, 1.4468, 1.4515, 1.4517, 1.4501, 1.4467, 1,4569, 1.4508
X2 CrNiMoCuN 25-6-3, X2 CrNiMoN 25-7-4, GX2 CrNiMoN 25-6-3, GX2 CrNiMoCuN 26-6-3, GX2 CrNiMoCuN 25-6-3-3, X2 CrNiMoCuWN 25-7-4, X2CrMnNiMoN26-5-4, X 2 CrNiMoN 26 7 4, GX2CrNiMoCuWN25-8-4
UNS S32520, S32550, S32750, S39274, S39277, S39553, S32760, J93380
Ferralium 255, SAF 2507, ZERON 100, UR 76 N, SM22Cr, SAF 2507, Alloy 2507, Alloy 2594
Heat Treatment |
RP0,2 (MPa) |
Rm (MPa) |
A5 (%) |
Impact Energy (J) ISO-V | Hardness | |
---|---|---|---|---|---|---|
RT | -40°C | |||||
As Welded | 620 | 820 | 20 | 70 | 55 | HRc |