Castolin XHD-6865
Latest generation high recovery type (170%) guarantees optimum deposit rate and metallurgical quality and attractive welder appeal in the PA-PB position. Very good resistance against pitting corrosion and crevice corrosion. Very good against acid, neutral or alkaline media, with or without chlorides. Very good resistance at high temperatures, especially against oxidation.
Ni 6625 / NiCr22Mo9Nb / 2.4831
W.Nr: 1.4529, 1.4539, 1.4547, 1.4876, 1.4958, 1.5656, 2.4660, 2.4816, 2.4856, 2.4858,
X1CrNiMoCuN20-18-7 - X10NiCrAlTi32-20 - X5NiCrAITi31-20 - NiCr15Fe - NiCr22Mo9Nb - NiCr21Mo - X1NiCrMoCuN25 20 6 - X1NiCrMoCuN25 20 5 - NiCr21Mo - 8XNi9
ASTM: A 533 Gr1, B443, B444, B446
UNS: S31254 - N08800 - N08810 - N06600 - N06625 - N08825 - N08926 - N08020
Alloy 254 SMO - Alloy 800 - Alloy 800H - Alloy 600 - Alloy 625 - Alloy 825 - Sanicro 28
Heat Treatment |
RP0,2 (MPa) |
Rm (MPa) |
A5 (%) |
Impact Energy (J) ISO-V | Hardness | |
---|---|---|---|---|---|---|
RT | -196°C | |||||
As Welded | 455 | 795 | 37 | 78 | 60 | HRc |