- spécifications du produit
- conditionnement
- demander un devis
There is no limit for the number of layers that can be applied in case of rebuilding but heat input should be kept low (as for Mn steel, interpass temperature should be kept < 250 °C).
Rebuilding and joining cold straining Mn steels or rebuilding parts that are subject to high impact and rolling wear. Breaker teeth, Crushers, Hammers, Crossings, Rails.
Heat Treatment |
RP0,2 (MPa) |
Rm (MPa) |
A5 (%) |
Hardness |
---|---|---|---|---|
As Welded | 270 HB |