De corrosieweerstand is hoger dan de vereisten voor 5%Cr-0,5%Mo staal. Te gebruiken met beschermgas Ar+O2.
9%Cr-1%Mo
1.7386, 1.7388, 1.7389
BS 3100 Gr B6, BS 3604 Gr CFS 629-470, HFS 629-470, BS 3604 Gr HFS 629-590, CFS 629-590, GS-12CrCrMo 10-1, X12CrMo 9-1, X7CrMo 9-1
ASTM: A182 Gr F9, A199 Gr T9 , A213 Gr T9 , A217 Gr C12 , A234 Gr WP9, A335 Gr 9, A336 Gr F9, A387 Gr 9,
Heat Treatment |
RP0,2 (MPa) |
Rm (MPa) |
A5 (%) |
Impact Energy (J) ISO-V | Hardness |
---|---|---|---|---|---|
RT | |||||
745°C±15°C 1h | 490 | 600 | 20 | 110 | HRc |