also SAW
CEWELD® SA 307 for tough buffer layers before hardfacing, 14% manganese steels, 13 - 17% chromium and heat-resistant steels and mixed compounds. Rails, as a buffer layer on concrete crushers
CEWELD® SA 307 for tough buffer layers before hardfacing, 14% manganese steels, 13 - 17% chromium and heat-resistant steels and mixed compounds. Rails, as a buffer layer on concrete crushers
CEWELD® SA 307 has a medium strength with very high resistance to cracking due to its high elongation. We recommend CEWELD® FL 838 or FL 880 as welding flux
19%Cr, 9%Ni Type, ISO 15608: 8.1 , 1.4316
1.4306, 1.4301, 1.4541, 1.4550, 1.4311, 1.4546, 1.4312, 1.4300, 1.4312, 1.4371, 1.4541, 1.4543, 1.4550, 1.4452
X2CrNi 19 11 (TP), X4CrNi 18 10 (TP), X6CrNiTi 18 10 (TP), X6CrNiNb 18 10 (TP), X2CrNiN 18 10 (TP), X5CrNiNb 18 10, G-X10CrNi 18 8 (TP)
AISI 202, 302, 304L, 304, 305, 321, 347, 304 LN,
ASTM A320 Grade B8C/D
Heat Treatment |
RP0,2 (MPa) |
Rm (MPa) |
A5 (%) |
Impact Energy (J) ISO-V | Hardness |
---|---|---|---|---|---|
RT | |||||
As Welded | 400 | 600 | 34 | 80 | HRc |
CEWELD 307Si is for buffer layers before hardfacing, dissimilar welding between steel and stainless steel, armor plate, exhaust systems (type 409, 304), high Manganese austenitic steel, heterogeneous welding, difficult to weld steels etc. The deposit work hardens from 200 HV to 450 HV.
CEWELD 307Si is for buffer layers before hardfacing, dissimilar welding between steel and stainless steel, armor plate, exhaust systems (type 409, 304), high Manganese austenitic steel, heterogeneous welding, difficult to weld steels etc. The deposit work hardens from 200 HV to 450 HV.
Corrosion resistance is equivalent to type 304, high mechanical properties and good weldability, work hardening and cold-tough to -196°C.
19% Cr / 9% Ni / 7% Mn, ISO 15608: 8.1 Cr ≤ 19 %
1.3401, 1.5637, 1.5680, 1.4370
X 20 Cr 13, X 8 Cr 17, X 22 CrNi 17, X 5 CrNi 17, G-X 20 Cr 14 mix S355
42CrMo4, C45, 42MnV7, X120Mn12, 10 Ni 14, 12 Ni 19 etc.
ASTM 307, 304, (409, 403, 405, 410, 420, 430, 440, 501, 502)
Amor
Heat Treatment |
RP0,2 (MPa) |
Rm (MPa) |
A5 (%) |
Impact Energy (J) ISO-V | Hardness |
---|---|---|---|---|---|
-196°C | |||||
As Welded | 400 | 600 | 40 | 40 | HRc |