- PRODUCT SPECIFICATIONS
- PACKAGING
- Ask quotation
Joining and cladding high heat resistant CrNi-steels of the same kind and Cast steels in a low sulphourus invironment. Typical alloy for welding of pyrolysis furnace tubes.
Joining and cladding high heat resistant CrNi-steels of the same kind and Cast steels in a low sulphourus invironment. Typical alloy for welding of pyrolysis furnace tubes.
Recommended for operating temperatures up to 1050°C in carburized invironments in ovens in petrochemical plants.
1.4876, 1.4859, 1.4958, 1.4959,
X10NiCrAlTi32-21, GX10NiCrSiNb32-20, X5NiCrAlTi31-20, X8NiCrAlTi32-21, X 12 CrNiTi 18 9
UNS N08800, N08810, N08811
Alloy 800, Alloy 800H, Alloy 800HT, Manaurite 900, Nicrofer 3220 H
Heat Treatment |
RP0,2 (MPa) |
Rm (MPa) |
A5 (%) |
Impact Energy (J) ISO-V | Hardness |
---|---|---|---|---|---|
RT | |||||
As Welded | 410 | 620 | 21 | 82 | HRc |