Type
Rutile basic Austenitic, non magnetic stainless steel electrode
classification
AWS
A 5.4: E ~317L-17
EN ISO
3581-A: E 18 16 5 L R 32
W.Nr.
1.4440
Toepassingen
For welding stabilized and un-stabilized CrNiMo(N) type of steels with high corrosion resistance. Also suitable for dissimilar welds between steel and stainless steel or dissimilar stainless steels. Mainly used in chemical, paper and cotton industry
Type
Rutile basic Austenitic, non magnetic stainless steel electrode
Toepassingen
For welding stabilized and un-stabilized CrNiMo(N) type of steels with high corrosion resistance. Also suitable for dissimilar welds between steel and stainless steel or dissimilar stainless steels. Mainly used in chemical, paper and cotton industry
Eigenschappen

High mechanical properties and excellent weldability, corrosion resistance is better than AISI 316 due to the high Mo. content. Suitable for use up to 400 °C. The weld deposit is non magnetic.

Classificatie
AWS
A 5.4: E ~317L-17
EN ISO
3581-A: E 18 16 5 L R 32
F-nr
4
FM
5
W.Nr.
1.4440
Geschikt voor

Designed for joining corrosion resistant CrNiMoN steel as well as for austenitic-ferritic joints.

ISO 15608: 8.1  Austenitic ≤ 19 % Cr , TÜV 1000: Gr. 26, 27, 28

1.4429, 1.4434, 1.4435, 1.4436, 1.4438, 1.4439, 1.4453, 1.4583, 

X2CrNiMoN 17 13 5, X2CrNiMoN 17 13 3, X2CrNiMo 18 15 4, X10CrNiMoNb 18 12, X2CrNiMoN17-13-3, X2CrNiMoN18-12-4, X2CrNiMo18-14-3, X3CrNiMnMoN19-16

UNS S31600, S31653, S31703, S31726, S31753

AISI 316Cb, 316L, 316LN, 317L, 317LN, 317LMN

Lasposities
PA
PB
PC
PD
PE
PF
Herdrogen
300°C / 2 hr
Analyse
C Si Mn P S Cr Ni Mo Nb N Cu Ta Nb+Ta W
0.03 0.8 1.1 0.02 0.015 19 13 3.8
Mechanische waarden
Heat
Treatment
RP0,2
(MPa)
Rm
(MPa)
A5
(%)
Impact Energy (J) ISO-V Hardness
RT
As Welded 400 580 32 70 HRc